Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 184 - 270 °C | 363 - 518 °F | |
Indium Corp. Indalloy 146 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 260 - 270 °C | 500 - 518 °F | |
Guarniflon FEP Fluorinated Ethylene Propylene Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t.. |
|||
Melting Point | 255 - 270 °C | 491 - 518 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA C920-0020X Perfluoroalkoxy (PFA) Hyflon® PFA C920-0020X is a semi crystalline, melt processable perfluoroalkoxy fluorocarbon resin specifically designed for applications where the unique properties of PFAs must be combined with .. |
|||
Melting Point | 250 - 270 °C | 482 - 518 °F | ASTM D-3418 |
Saint-Gobain Norton® ETFE Fluoropolymer Film Features/Benefits:Superior release propertiesExcellent weatherabilityPerformance from -200°C (-328°F) to 165°C (330°F)Excellent chemical and mechanical propertiesThermoformableProduct th.. |
|||
Melting Point | 220 - 270 °C | 428 - 518 °F | |
Tisan TISBLEND® PC/ABS TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High.. |
|||
Melting Point | 260 - 270 °C | 500 - 518 °F | |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Melting Point | 260 - 270 °C | 500 - 518 °F | |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |