Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 247 - 249 °C | 477 - 480 °F | |
Sibur TVERPET® Polyethylene Terephthalate (PET) For production of polyether fibers and threads, different kinds of technical and medical films, plastic bottles, packing for food products and domestic chemistry. Mineral and drinking water, non-ga.. |
|||
Melting Point | 243 - 249 °C | 469 - 480 °F | |
Ex-Tech Plastics VersaTech™ PET Ex-Alloy 3400, 100% Post Consumer FDA, RPET Extruded Sheet Delivering all the qualities of PET, this sheet is developed using post consumer material, allowing the packaging to carry marketing reference terms such as sustainability, green and recycled.Charac.. |
|||
Melting Point | 232 - 249 °C | 450 - 480 °F | ASTM D789 |
Adell WR-37 33% Glass Reinforced PET |
|||
Melting Point | 232 - 249 °C | 450 - 480 °F | ASTM D789 |
Adell WL-38 40% Glass and Mineral Reinforced PET |