Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 103 - 227 °C | 217 - 441 °F | |
Indium Corp. Indalloy 217-440 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax CCP PBT 1100-211X Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 183 - 227 °C | 361 - 441 °F | |
Indium Corp. Indalloy 125 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 215 - 227 °C | 419 - 441 °F | |
Indium Corp. Indalloy 258 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 217 - 227 °C | 423 - 441 °F | |
Indium Corp. Indalloy® 263 Tin-Silver-Copper Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211XG Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 220 - 227 °C | 428 - 441 °F | DSC |
Solvay Specialty Polymers Halar® 6012F Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® 6012F is semi-crystalline fluoropolymer designed specifically for rotational molding and lining. Rotomolding is typically used to manufacture articles such as tanks, bottles and vessels wh.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211MB Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 225 - 227 °C | 437 - 441 °F | Average value: 227 °C Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |