Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 191 - 201 °C | 376 - 394 °F | |
UBE 5033B Air Blown Nylon 6/66 Film Specialties: Standard nylon 6/66Medium shrink, Low slipApplications: Best for Middle layer usageProcessing: Top web (Air blown)Thermoforming (T-die)Information provided by UBE. |
|||
Melting Point | 191 - 201 °C | 376 - 394 °F | |
UBE 5033FDX27 Air Blown Nylon 6/66 Film Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE. |