Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1.. |
|||
Melting Point | 120 - 165 °C | 248 - 329 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding .. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ASTM D789 |
Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ASTM D789 |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HB300BF Polypropylene Homopolymer for Capacitor Film Borclean HB300BF is a homopolymer film resin developed for use in the manufacture of the highest quality films or dielectric applications. Borclean HB300BF does not contain slip, antiblock, antista.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film Borclean HB311BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HB311BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC300BF Polypropylene Homopolymer for Capacitor Film Borclean HC300BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC300BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC314BF Polypropylene Homopolymer for Capacitor Film Borclean HC314BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC314BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC320BF Polypropylene Homopolymer for Capacitor Film Borclean HC320BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC320BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 162 - 165 °C | 324 - 329 °F | DSC; ISO 3146 |
Borealis HB205TF Polypropylene HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | DSC; ISO 3146 |
Borealis HC401BF Polypropylene Homopolymer HC401BF is a polypropylene homopolymer. Applications HC401BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, package.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis HF420FB Polypropylene HF420FB is a polypropylene homopolymer intended for fiber applications. HF420FB has been developed especially for applications like: staple fiber, continuous filaments, and spun bonded nonwovens.In.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet TOTAL Petrochemicals Polypropylene 4252 is a 1.5 melt flow rate impact copolymer designed for improved toughness and high melt strength. This resin offers outstanding processability in combination .. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | DSC |
Total PPC 4481WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4481WZ is a nucleated impact copolymer with a Melt Flow index of 4.0 g/10 min.TOTAL Polypropylene 4481WZ is characterized by a good stiffness/impact balance couple.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 4720XWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ATOFINA Method |
Total PPC 4824WZ Polypropylene, Impact Copolymer ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent .. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | TOTAL Method |
Total PPC 4944CWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4944CWZ is a nucleated and controlled rheology impact copolymer with a very high Melt Flow index of 50 g/10 min.TOTAL 4944CWZ is characterized by improved stiffnes.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP10 GR10 NL PPCP, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 BK EC PPCP, conductive, black Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 GR40 NL PPCP, 40% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP20 MF20 NL XA70 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 301-F Polyvinylidene Fluoride Powder Characteristics: Fine milled, white, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abra.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | DSC |
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 135 - 165 °C | 275 - 329 °F | Average value: 157 °C Grade Count:8 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |