Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 149 - 157 °C | 300 - 315 °F | |
Plaskolite Optix® Acrylic Sheet Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,.. |
|||
Melting Point | 149 - 157 °C | 300 - 315 °F | |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |
|||
Melting Point | 132 - 157 °C | 270 - 315 °F | Average value: 150 °C Grade Count:7 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |