Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 130 - 134 °C | 266 - 273 °F | ASTM D3418 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Melting Point | 130 - 134 °C | 266 - 273 °F | ISO 3146 |
Borealis Borseal™ TD120BF Terpolymer for BOPP Film Borseal TD120BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD120B.. |
|||
Melting Point | 130 - 134 °C | 266 - 273 °F | ISO 3146 |
Borealis Borseal™ TD220BF Terpolymer for BOPP Film Borseal TD220BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD220B.. |