Polymer Property : Melting Point = 2540 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1340 - 1390 °C
2450 - 2540 °F
Carlson 330 Austenitic Alloy
General DescriptionCarlson Alloy 330 is a nickel-iron-chromium-silicon austenitic alloy. It combines high strength with excellent resistance to carburization and oxidation at temperatures to 2200°..