Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 106 - 116 °C | 223 - 241 °F | |
Oceanchem Group Bis (2,3-dibromopropyl ether) of TBBA (BDDP) Molecular Formula: C21H20Br8O2Cas No.: 21850-44-2Application: BDDP used for plastics as flame-retardant, is designed for use in PP (homopolymer and copolymer) and high impact polystyrene (HIPS) appl.. |