Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 71.0 - 88.0 °C | 160 - 190 °F | TMA Melt Range |
Huntsman IROGRAN® PS 456-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Melting Point | 80.0 - 88.0 °C | 176 - 190 °F | |
M Chemical GUARD DOGâ„¢ UV328 Benzotriazole UV Absorber GUARD DOGâ„¢ UV328 light stabilizer is a derivative of Benzotriazole that has exceptionally strong and broad-range UV absorption properties throughout the UV spectrum specially designed for polym.. |
|||
Melting Point | 78.0 - 88.0 °C | 172 - 190 °F | |
Fine Organics FINALUX G 621 Lubricant Additive Applications: Compatible external lubricant with strong effet suitable for rigid PVC calendered films, fittings, bottles etc.Information provided by Fine Organics |
|||
Melting Point | 71.0 - 88.0 °C | 160 - 190 °F | |
Indium Corp. Indalloy 160-190 Fusible Bismuth Alloy Information Provided by Indium Corporation |
|||
Melting Point | 78.0 - 88.0 °C | 172 - 190 °F | |
Fine Organics FINAWAX E Lubricant Additive Applications: Slip additive for polyolefins, also suggested in artificial leather to achieve dry feel, release agent for plastisols.Information provided by Fine Organics |
|||
Melting Point | 47.0 - 88.0 °C | 117 - 190 °F | ASTM D3418(DSC) |
DuPont Surlyn® 8945 Thermoplastic Ionomer Resin Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer sp.. |