Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 70.0 - 73.0 °C | 158 - 163 °F | |
Indium Corp. Indalloy 22 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 73.0 °C | 158 - 163 °F | |
Indium Corp. Indalloy 23 Bismuth Solder Alloy Non-electrical solder for low-ambient temperatureInformation Provided by Indium Corporation |
|||
Melting Point | 70.0 - 73.0 °C | 158 - 163 °F | |
Indium Corp. Indalloy 24 Bismuth Solder Alloy Information Provided by Indium Corporation |