Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 68.0 - 72.0 °C | 154 - 162 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 102 Linear Thermoplastic Polyurethane PEARLBOND® 102 is a linear, polycaprolactone-based polyurethane, supplied in form of small white pellets, which combines a very high crystallization rate with a very high thermoplasticity level.A.. |
|||
Melting Point | 68.0 - 72.0 °C | 154 - 162 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 502 Linear Thermoplastic Polyurethane PEARLBOND™ 502 is a linear, polycaprolactone-copolyester polyurethane with a high crystallization rate and a very high thermoplasticity level.Application: Pearlbond™ 502 can be added to fo.. |
|||
Melting Point | 69.0 - 72.0 °C | 156 - 162 °F | |
Suqian Unitechem Efficient Inhibitor 701 Chemical Name: 4-Hydroxy-2,2,6,6-tetramethyl-piperidinooxy (TMHPO')CAS NO.: 2226-96-2Molecular Formula: C9H18NO2Uses: It can prevent alkene from self-polymerization, or control and adjust the degree.. |
|||
Melting Point | 65.0 - 72.0 °C | 149 - 162 °F | |
BASF Diisopropanol-p-toluidine Formula: C13H21NO2CAS: 38668-48-3Description: Diisopropanol-p-toluidine is a colorless to yellowish paste with and amine-like odor. This product is only sparingly soluble in water.Synonyms: DIIPT, .. |