Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 830 - 850 °C | 1530 - 1560 °F | |
Wieland 1408 Wilaform Gold Hard yellow gold alloy. Easily splintered and polished.Applications: casting, laminar decoration, tubingDental |
|||
Melting Point | 750 - 850 °C | 1380 - 1560 °F | |
Williams Advanced Alloys Wambraze™ WB850 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |