Thermal Properties Metric English Comments
Melting Point 58.0 - 60.0 °C
136 - 140 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® DIPP-539 is a linear, polycaprolactone-copolester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® DIPP-539 can be adde..
Melting Point 50.0 - 60.0 °C
122 - 140 °F
Fine Organics FINALUX G 301 Lubricant Additive
Applications: Compatible all round lubricant for rigid PVC extrusion/molding.Information provided by Fine Organics
Melting Point 50.0 - 60.0 °C
122 - 140 °F
Fine Organics FINALUX G 531 Lubricant Additive
Applications: Internal lubricant for rigid PVC extrusion and injection molding.Information provided by Fine Organics
Melting Point 50.0 - 60.0 °C
122 - 140 °F
Fine Organics FINALUX G 701 Lubricant Additive
Applications: Highly effective release agent for rigid PVC, for use in calendered films/rigid PVC fittingsInformation provided by Fine Organics
Melting Point 50.0 - 60.0 °C
122 - 140 °F
Fine Organics FINALUX G 741 Lubricant Additive
Applications: Excellent release agent like G 701 for rigid PVC films, but with more compatibility, also suggested for Sn-stabilized RPVC fittings.Information provided by Fine Organics
Melting Point 55.0 - 60.0 °C
131 - 140 °F
Shandong Dongyue Shenzhou New Material Co Perfluorooctanoic Acid (PFOA)
Conformable with: Q/DYS 006-2007PFOA is a strong organic acid, which has low surface tension and high surface activity, being used as surfactant, dispersant and additive. PFOA and its derivatives a..
Melting Point 58.0 - 60.0 °C
136 - 140 °F
MQSA 70A
Lubrizol Advanced Materials Pearlbond® 539 Thermoplastic Polyurethane
Pearlbond® 539 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl..