Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 657.2 - 688 °C | 1215 - 1270 °F | |
Lucas-Milhaupt FOS FLO 670 Copper Phosphorus Tin Braze Filler Metal Applications:Fos-Flo 7 iFos-Flo 670 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encounter.. |
|||
Melting Point | 646.1 - 688 °C | 1195 - 1270 °F | |
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu.. |
|||
Melting Point | 632 - 688 °C | 1170 - 1270 °F | |
Lucas-Milhaupt EASY FLO 3 Carbide Brazing Alloy Easy-Flo 3 is recommended for use on stainless steels subject to chloride corrosion, such as marine hardware, fishing tackle, and some dairy equipment cleaned with bleaching solutions and other equi.. |
|||
Melting Point | 632 - 688 °C | 1170 - 1270 °F | |
Lucas-Milhaupt Silvaloy® 50N Brazing Alloy Silvaloy 50N is a modification of Silvaloy 50. It was originally introduced because of somewhat better corrosion resistance than Silvaloy 50 for certain conditions, and is still used for such purpos.. |
|||
Melting Point | 632 - 688 °C | 1170 - 1270 °F | |
Universal Wire Works BAg-3 (AMS 4771) Silver Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 630 - 690 °C | 1170 - 1270 °F | |
Indium Corp. Indalloy 218 Silver Solder Alloy Information Provided by Indium Corporation |