Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 43.0 - 53.0 °C | 109 - 127 °F | |
Fine Organics FINALUX G 602 Lubricant Additive Applications: Universal internal lubricant for rigid PVC and foamed PVC, applicable independently of stabilizing system. Pseudo-plasticizer for PVC. Low improver and lubricant for PMMAInformation .. |