Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 451 - 465 °C | 844 - 869 °F | |
Indium Corp. Indalloy 177 Gold-Indium Solder Alloy Extremely hard, high temperature alloyInformation Provided by Indium Corporation |
|||
Melting Point | 451 - 485 °C | 844 - 905 °F | |
Indium Corp. Indalloy® 178 Au-In Solder Alloy Extremely hard, high temperature alloy. Stiff alloy.Information provided by the manufacturer, Indium Corporation. |