Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 313 °C | 595 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications... |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Melting Point | 313 °C | 595 °F | ASTM D570 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Melting Point | 313 °C | 595 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Melting Point | 313 °C | 595 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, at 50% RH
&n AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Melting Point | 313 °C | 595 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Melting Point | 313 °C | 595 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, at 50% RH
(disc AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Melting Point | 313 °C | 595 °F | Eutectic |
Indium Corp. Indalloy® 239 Pb-Ag-Sn-In Solder Alloy High temp solder.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Melting Point | 313 °C | 595 °F | DSC |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Melting Point | 313 °C | 595 °F | Dry; ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Melting Point | 313 °C | 595 °F | Dry; DSC |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Melting Point | 313 °C | 595 °F | DSC |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Conditioned, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Conditioned, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Conditioned, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Melting Point | 313 °C | 595 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |