Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 305 °C | 581 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data) Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop.. |
|||
Melting Point | >= 305 °C | >= 581 °F | |
Hong Kun Group UV Absorber CAS No. 1163-19-5All information provided by Hongkun Group |
|||
Melting Point | 305 - 364 °C | 581 - 687 °F | |
Indium Corp. Indalloy 175 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 305 °C | 581 °F | Peak; Dry; ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Melting Point | 305 °C | 581 °F | Dry; ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Melting Point | 305 °C | 581 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Melting Point | 305 °C | 581 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Melting Point | 305 °C | 581 °F | |
ScanTube PFA Tubing Information provided by ScanTube, Inc. |
|||
Melting Point | 305 - 315 °C | 581 - 599 °F | |
Asahi Glass Fluon® P-66P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 305 - 315 °C | 581 - 599 °F | |
Asahi Glass Fluon® P-63P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 305 - 315 °C | 581 - 599 °F | |
Asahi Glass Fluon® P-65P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 305 - 315 °C | 581 - 599 °F | |
Asahi Glass Fluon® P-802UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 305 - 315 °C | 581 - 599 °F | |
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 305 - 315 °C | 581 - 599 °F | |