Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 245 °C | 473 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Melting Point | 245 °C | 473 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Melting Point | 245 - 247 °C | 473 - 477 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Melting Point | 245 °C | 473 °F | ISO 11357-1 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Melting Point | 245 °C | 473 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Custom Resins Vexel™ E20GF30 , 30% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF30 is a 30% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Custom Resins Vexel™ E20MG35 , 35% Glass/Mica Reinforced PET
(discontinued **) Description: Vexel™ E20MG35 is a 20% glass fiber / 15% mica reinforced PET. Information provided by Custom Resins. |
|||
Melting Point | 245 - 247 °C | 473 - 477 °F | |
SK Chemicals SKYPET® XT8050 Specially Formulated PET Copolymer Resin Description: SKYPET-XT8050 is a fast reheat grade of SKYPET, specially formulated for high productivity in the blowing process. SKYPET-XT8050 provides excellent processability in injection molding .. |
|||
Melting Point | 245 °C | 473 °F | ISO 3146 |
Wellman Wellpet® PR109-N1 Unfilled PET Description: Unfilled PETInformation provided by Wellman. |
|||
Melting Point | 245 °C | 473 °F | ISO 3146 |
Wellman Wellpet® PR118-N2 Unfilled Polyester PET Description: Unfilled Polyester PETInformation provided by Wellman. |
|||
Melting Point | <= 245 °C | <= 473 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Melting Point | <= 245 °C | <= 473 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper.. |
|||
Melting Point | 245 - 255 °C | 473 - 491 °F | |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 110 BK-112 15% Glass Filled PET Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 130 FR 30% Glass Filled PET Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail.. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 130 FR 30% Glass Filled PET Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
BASF Petra® 7010 BK 5830 15% Glass Filled PET Description: Petra 7010 BK5830 is a 15% glass fiber reinforced, pigmented black injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
BASF Petra® 7010 WT 7729 15% Glass Filled PET Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 7030 GY6128 30% Glass Filled PET Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It o.. |
|||
Melting Point | 245 °C | 473 °F | ISO 11357-1 |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Melting Point | 245 °C | 473 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVAMID 66/6 GF 30 Polyamide 66/6, 30% Glass Fiber
(discontinued **) FeaturesChemically reinforced alloy PA 66 and PA 6 with 30% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and el.. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |
|||
Melting Point | 245 - 255 °C | 473 - 491 °F | Average value: 251 °C Grade Count:25 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Melting Point | 245 °C | 473 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Ashley Polymers Ashlene® PE128 PET Polyester, 45% Glass Reinforced PET Polyester, with 45% glass reinforcement.Data provided by the manufacturer |