Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 240 °C | 464 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Melting Point | 240 °C | 464 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet) |
|||
Melting Point | 240 °C | 464 °F | ISO 11357-3 |
Pasargad Polymer Peyvand Pasalac 3P-H6000B ABS Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Melting Point | 240 °C | 464 °F | |
Plastcom SLOVASTER® C FRU 2 PBT, flame retarder FeaturesPC with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other hole products. Application in engineer.. |
|||
Melting Point | 240 °C | 464 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman PG400 PET
(discontinued **) Voridian PET PG400 is a general purpose resin is mostly supplied into Mexico and has a wide array of applications in container manufacturing.Applications/UsesBeverage packagingContainersFood packagi.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Melting Point | 240 °C | 464 °F | MPC Method |
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade
(discontinued **) TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Melting Point | 240 °C | 464 °F | C-120 |
I. Stern IS-7985 Polyethylene Terephthalate Resin Product Description: IS-7985 is a natural polyethylene terephthalate (PET) resin. This resin is produced by continuous melt phase polymerization followed by solid phase polymerization.Certificatio.. |
|||
Melting Point | 240 °C | 464 °F | ASTM D-3418 |
Saint-Gobain Norton® PMP Film Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail.. |
|||
Melting Point | >= 240 °C | >= 464 °F | BD-61305 |
Wellman AquaClear® Ti844 PET AquaClearTI® 844 is a TPA-based polyethylene terephthalate resin made especially for use in the packaging applications. It’s a solid state copolymer resin with an intrinsic viscosity of 0.72. Aqua.. |
|||
Melting Point | >= 240 °C | >= 464 °F | |
Wellman PermaClear™ 61803 (0.81 IV) PET PermaClear® 61803 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.81 IV. PermaC.. |
|||
Melting Point | >= 240 °C | >= 464 °F | BD-61305 |
Wellman PermaClear™ HP806 (0.84 IV) PET PermaClear® HP806 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.84 IV. PermaC.. |
|||
Melting Point | 240 °C | 464 °F | BD-61305 |
Wellman ThermaClear® Ti818 (0.79 IV) PET ThermaClearTI® Ti818 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. Its titanium catalyst and copolymer formulation provide outstanding clarity a.. |
|||
Melting Point | 240 - 264 °C | 464 - 507 °F | |
Williams Advanced Alloys WS264 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 240 °C | 464 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman Aqua PJ002 PET Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer PJ.. |
|||
Melting Point | 240 °C | 464 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® HS Ti818 (G51A) PET Laser+® HS Ti818 (G51A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technology.Laser+® HS Ti818 (.. |
|||
Melting Point | 240 °C | 464 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® W Ti844 P46A PET Product Description: Laser+® W Ti844 (P46A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology... |
|||
Melting Point | >= 240 °C | >= 464 °F | |
Ex-Tech Plastics VersaTech™ APET Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.Characteristics:TransparentExcepti.. |
|||
Melting Point | 240 °C | 464 °F | DIN 53765 |
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Melting Point | 240 °C | 464 °F | DIN 53765 |
BASF Ultramid® C3U10 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Melting Point | 240 °C | 464 °F | DIN 53765 |
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Dry) Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire .. |
|||
Melting Point | 240 °C | 464 °F | DIN 53765 |
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Conditioned) Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire .. |
|||
Melting Point | 240 °C | 464 °F | MPC Method |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |