Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF15 , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 is a 15% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF15 FR , 15% Glass Reinforced, Flame Retardant PBT Description: Vexel™ B12GF15 FR is a 15% glass fiber reinforced flame retardant PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polyme.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF15 SA , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 SA is a 15% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF30 , 30% Glass Reinforced PBT Description: Vexel™ B12GF30 is a 30% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF30 FR , 30% Glass Reinforced, Flame Retardant PBT Description: Vexel™ B12GF30 FR is a 30% glass fiber reinforced, flame retardant PBT. B12GF30 FR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all .. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF30 SA , 30% Glass Reinforced PBT Description: Vexel™ B12GF30 SA is a 30% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF45 , 45% Glass Reinforced PBT Description: Vexel™ B12GF45 is a 45% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12GF45 SA , 45% Glass Reinforced PBT Description: Vexel™ B12GF45 SA is a 45% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B12U FR Un-reinforced, Flame Retardant PBT Description: Vexel™ B12U FR is an un-reinforced, flame retardant PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources .. |
|||
Melting Point | 227 °C | 440 °F | ASTM D3418 |
Nylene® Vexel™ B50U , High Flow, Un-reinforced PBT Description: Vexel™ B50U is a high flow, un-reinforced PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Melting Point | 227 - 238 °C | 440 - 460 °F | |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Melting Point | 227 - 238 °C | 440 - 460 °F | |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |