Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 224 °C | 435 °F | |
Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre Features: PBT for injection moulding, chemically reinforced with 40% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
Nylene® 8100 Unfilled Nylon 6/12 Description: Nylene® 8100 is an unfilled specialty fiber. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
Nylene® 9543 , 43% Glass Reinforced Nylon 6/12 Description: Nylene® 9543 s a 43% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour.. |
|||
Melting Point | 224 - 229 °C | 435 - 444 °F | |
Oceanchem Group Antioxidant 1024 Molecular Formula: C34H52N2O4Uses: Dosage is 0.1-0.5 portions. It is a metal deactivator, can work with antioxidant, used in PE, PP, polystyrene, polyamnamee, polyester, or used as antioxidant of b.. |
|||
Melting Point | 224 °C | 435 °F | ISO 3146 |
PolyOne Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melting Point | 224 °C | 435 °F | ISO 3146 |
PolyOne Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® S610SF BK851 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP210 General Purpose PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP212VO Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP2122G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP513FLBL Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP212G15V0BM G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, paintabilityApplications: A variety of cases and connectorsInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G15BL Glass Fiber Reinforced PBT Compound Resin b>Characteristics: G/F 15% reinforced, BLACKApplications: Impeller housingsInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Pocan® DP 2004 000000 PBT PBT, non-reinforced, injection molding, halogen free flame retardant |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
Melting Point | 224 °C | 435 °F | |
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearance: BlackTPCI# .. |
|||
Melting Point | 224 °C | 435 °F | DSC Peak; JIS K7121 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Melting Point | 224 °C | 435 °F | ISO 11357-1/-3 |
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Melting Point | 224 °C | 435 °F | ASTM DSC |
Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, Dry As Molded Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® S610SF BK851 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
Melting Point | 224 °C | 435 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation .. |
|||
Melting Point | 224 °C | 435 °F | ISO 3146 |
Azoty Tarnow™ Alphalon™ E 40 T Nylon 6 A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™ |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
(Unverified Data**) Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**) Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia.. |