Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 219 °C | 426 °F | ASTM D789 |
NYCOA 1417HS PA 6 impact modified, heat stabilized, medium high impact strengthInformation provided by NYCOA, Inc. |
|||
Melting Point | 219 °C | 426 °F | |
Oxford Polymers Oxnilon 6-14GF 14% Glass Fiber Filled Nylon 6 for Injection Molding 14% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Melting Point | 219 °C | 426 °F | |
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding 33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Melting Point | 219 °C | 426 °F | |
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding 43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided .. |
|||
Melting Point | 219 °C | 426 °F | Peak |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
Melting Point | 219 °C | 426 °F | ASTM D3418 |
SK Chemicals SKYPEL P147D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade) Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right bal.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 219 °C | <= 426 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: .. |
|||
Melting Point | 219 °C | 426 °F | ASTM D3418 |
Ashley Polymers Ashlene® 982 Nylon 612 General purpose for extrusion. These resins are notes for their low moisture absorption and excellent dimensional stability. Bristle grade, high viscosity.Data provided by the manufacturer |
|||
Melting Point | 219 °C | 426 °F | ASTM D3418 |
Ashley Polymers Ashlene® 990L-40G Nylon 610, 40% Glass Reinforced 40% glass reinforced, excellent dimensional stability and low water absorption. Also available as: 990LS-40G, same with heat stabilizer.Data provided by the manufacturer |
|||
Melting Point | 219 °C | 426 °F | ASTM D789 |
Chem Polymer Durlex 709 IH PBT, Impact Modified A highly impact modified PBT exhibiting excellent toughness and processability.Data provided by the manufacturer, Chem Polymer. |
|||
Melting Point | 219 °C | 426 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Pocan® DP C 1502 702353 PBT+PC
(discontinued **) PBT+PC, non-reinforced, injection molding, impact modified, low tendency to warp, UV-stabilized |
|||
Melting Point | 219 °C | 426 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612