Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 183 - 183 °C | 361 - 362 °F | |
Indium Corp. Indalloy 213 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 193 °C | 361 - 379 °F | MQSA 114 |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Melting Point | 183 °C | 361 °F | |
Lucas-Milhaupt 63 Sn-37 Pb Tin/ Silver Solder Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is desired. This allo.. |
|||
Melting Point | 183 - 192 °C | 361 - 378 °F | |
Indium Corp. Indalloy 110 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 222 °C | 361 - 432 °F | |
Indium Corp. Indalloy 122 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 238 °C | 361 - 460 °F | |
Indium Corp. Indalloy 130 Tin-Lead Solder Alloy Inexpensive utility solderInformation Provided by Indium Corporation |
|||
Melting Point | 183 - 247 °C | 361 - 477 °F | |
Indium Corp. Indalloy 135 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 187 °C | 361 - 369 °F | |
Suqian Unitechem Antioxidant 168 Chemical Name: Tris-(2,4-di-tert-butyl-phenyl)-phosphiteCAS NO.: 31570-04-4Molecular Formula: C42H63O3PProperties: The product takes on an appearance of white powder, without odor and smell. Solubl.. |
|||
Melting Point | 183 - 205 °C | 361 - 401 °F | |
Williams Advanced Alloys WS205 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 183 - 238 °C | 361 - 460 °F | |
Williams Advanced Alloys WS238 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 183 - 280 °C | 361 - 536 °F | |
Williams Advanced Alloys WS280 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 183 °C | 361 °F | |
Goodfellow Tin 60/Lead 39/Antimony 1 Alloy A general purpose, low melting point soft solder which can also be used as a protective coating and for metal film capacitors.Information provided by Goodfellow. |
|||
Melting Point | <= 183 °C | <= 361 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
Melting Point | <= 183 °C | <= 361 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00119 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Melting Point | 183 °C | 361 °F | DIN 53 736 |
Hippe PA 11 Nylon 11 Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorpti.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability .. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Conditioned) Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMV Nylon 11 (Dry) Designation ISO 1874-PA11,M,18-010Rigid grade for injection molding. Available color: natural. Free additive.High impact strength. Easy filling of the mold due to its well adapted melt viscosity. Lo.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BECN P20 TL Nylon 11 (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Dry) Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability .. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BECN W3 TL Nylon 11, Sheathing Grade (Dry) Designation ISO 1874-PA11,KFHL,12-010Rigid grade for sheathing wires and cables. Available color: natural. Light and heat stabilized. Flame retardant agent.Fire-resistant. High abrasion resistance. .. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Conditioned) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BESN P20 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-004Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.Flexibility. High impact strength. Very good chemical resistan.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Dry) Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc.. |
|||
Melting Point | 183 °C | 361 °F | ASTM D3417- ISO 3146 |
DuPont Surlyn® PC2000
(discontinued **) DuPont™ Surlyn® PC2000 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA c.. |
|||
Melting Point | 183 - 190 °C | 361 - 374 °F | |
Johnson Matthey JM6040 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |