Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 181 - 290 °C | 358 - 554 °F | Average value: 217 °C Grade Count:3 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melting Point | 181 °C | 358 °F | |
Noltex Soarnol® MS3203 Ethylene Vinyl Alcohol Copolymer Modified DC3203; New improved thermoformable EVOH. Ethylene content 32 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon .. |
|||
Melting Point | 181 °C | 358 °F | DSC |
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan.. |
|||
Melting Point | 181 °C | 358 °F | DSC |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
Melting Point | 181 - 187 °C | 358 - 369 °F | |
Indium Corp. Indalloy 226 Tin Solder Alloy Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation |
|||
Melting Point | 181 °C | 358 °F | DSC |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Melting Point | <= 181 °C | <= 358 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excelle.. |
|||
Melting Point | <= 181 °C | <= 358 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 15019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot.. |
|||
Melting Point | 181 °C | 358 °F | ASTM D3418 |
ALM PA 250 Nylon 12 SLS Prototyping Polymer Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or.. |
|||
Melting Point | 181 °C | 358 °F | ASTM D3418 |
ALM PA 605-A Filled Nylon 12 Prototyping Polymer 50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a.. |
|||
Melting Point | 181 °C | 358 °F | ASTM D3418 |
Ashley Polymers Ashlene® PPO Resin P259 A high flow grade for applications requiring high impact strength and a high heat deflection temperature.Data provided by the manufacturer |
|||
Melting Point | 181 °C | 358 °F | ASTM D3418 |
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe.. |
|||
Melting Point | 181 °C | 358 °F | ASTM D3418 |
ALM PA 650 Nylon 12 SLS Prototyping Polymer Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines.. |
|||
Melting Point | 181 °C | 358 °F | DSC |
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ.. |
|||
Melting Point | 181 °C | 358 °F | DSC |
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro.. |
|||
Melting Point | 181 °C | 358 °F | ASTM D3418 |
Ashley Polymers Ashlene® P258 PPO A high flow grade for applications requiring good impact strength and a high heat deflection temperature.Data provided by the manufacturer |