Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 175 °C | 347 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet) |
|||
Melting Point | 175 °C | 347 °F | Flow temperature, ASTM D569 |
Rotuba H5 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Melting Point | 175 °C | 347 °F | DSC |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Melting Point | 175 °C | 347 °F | DSC |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Melting Point | 175 - 178 °C | 347 - 352 °F | Average value: 177 °C Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melting Point | 175 °C | 347 °F | DIN 53736 |
Isoflon POM H Polyacetal H Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Melting Point | 175 °C | 347 °F | DSC |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Melting Point | 175 °C | 347 °F | |
Polyram PlusTek RD104 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melting Point | 175 °C | 347 °F | |
Polyram PlusTek RD120 Nylon 12, Injection Molding Polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 175 - 187 °C | 347 - 369 °F | |
Williams Advanced Alloys WS187 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE. |
|||
Melting Point | 175 °C | 347 °F | ISO 11357 |
Polyram PlusTek PD1002NT Nylon 12 for Extrusion Medium viscosity Nylon 12 for extrusion application.Information provided by Polyram. |
|||
Melting Point | 175 °C | 347 °F | ISO 11357 |
Polyram PlusTek PD120BK11 Nylon 12 for Extrusion, UV Stabilized Nylon 12 UV stabilized for extrusion application.Information provided by Polyram. |
|||
Melting Point | 175 °C | 347 °F | ISO 11357 |
Polyram PlusTek PD300G5 Nylon 12 for Injection Molding, 25% Glass-Fiber Reinforced 25% Glass-fiber reinforced Nylon 12, heat stabilized and hydrolysis resistant for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 175 °C | 347 °F | |
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 175 °C | 347 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM) DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a varie.. |
|||
Melting Point | 175 °C | 347 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Light ProtectionInformation provided by DuPont Performance Polymers |
|||
Melting Point | 175 °C | 347 °F | (Dry) |
Arkema Group Rilsan® BMV 400 TL Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,18-002,ZFlexible grade for injection molding. Available color: natural. Light and heat stabilized. Plasticizing agent free.Outstanding impact strength and tear spreading .. |
|||
Melting Point | 175 °C | 347 °F | 10°C/min |
Arkema Group Rilsan® BMV 400 TL Nylon 11 (Dry) Designation ISO 1874-PA11,M,18-002,ZFlexible grade for injection molding. Available color: natural. Light and heat stabilized. Plasticizing agent free.Outstanding impact strength and tear spreading .. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ashley Polymers Ashlene® RH190-PF Acetal, PTFE Filled A wear-resistant grade homopolymer resin with 1.5% PTFE.Data provided by the manufacturer |
|||
Melting Point | 175 - 195 °C | 347 - 383 °F | DSC Induction Temperature; TM-029 |
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Melting Point | 175 °C | 347 °F | (Dry) |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |
|||
Melting Point | 175 - 191 °C | 347 - 376 °F | Average value: 183 °C Grade Count:31 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melting Point | 175 °C | 347 °F | ASTM D3418 |
Ashley Polymers Ashlene® RH190H Acetal General purpose reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated RH190H-.. |
|||
Melting Point | 175 °C | 347 °F | DSC |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |