Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 168 °C | 334 °F | |
Polikim POLITAL® Polyoxymethylene (POM) Polital® is completely resistant to solvents, petroleum products, oil and grease. It is not resistant to strong acids, bases and oxidants. As it is affected by UV rays, its use in open air is not r.. |
|||
Melting Point | 168 °C | 334 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal
(Unverified Data**) Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such.. |
|||
Melting Point | 168 °C | 334 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal
(Unverified Data**) Delrin® FG400XRD NC010 is a filled, medium viscosity acetal copolymer for injection molding. It is detected in x-ray detectors. It has been developed for consideration into applications such as par.. |
|||
Melting Point | 168 °C | 334 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Melting Point | 168 - 178 °C | 334 - 352 °F | Average value: 174 °C Grade Count:14 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Melting Point | 168 °C | 334 °F | |
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 168 °C | 334 °F | ISO 11357 |
Polyram RamOfin PPH343T4BK10 Polypropylene, 20% Mineral Filled 20% Mineral filled, heat resistant polypropylene for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 168 °C | 334 °F | ISO 11357 |
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 168 °C | 334 °F | ISO 11357 |
Polyram RamOfin PPH343T8 Polypropylene, 40% Mineral Filled 40% Mineral filled polypropylene for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 168 °C | 334 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal (POM)
(Unverified Data**) X-ray Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400XRD NC010 is a filled medium viscosity acetal copolymer for injection molding. It is detected i.. |
|||
Melting Point | 168 °C | 334 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**) Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det.. |
|||
Melting Point | 168 °C | 334 °F | ASTM D3418 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Melting Point | 168 °C | 334 °F | (Dry) |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Melting Point | 168 °C | 334 °F | 10°C/min |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Melting Point | 168 °C | 334 °F | (Dry) |
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Melting Point | 168 °C | 334 °F | 10°C/min |
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Melting Point | 168 °C | 334 °F | DIN 53765 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Melting Point | 168 °C | 334 °F | ASTM D3418 |
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 32008/0009 is an ultra-flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 32008/0009 also has a very low brittleness te.. |
|||
Melting Point | 168 °C | 334 °F | (Dry) |
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |
|||
Melting Point | 168 °C | 334 °F | 10°C/min |
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |
|||
Melting Point | 168 °C | 334 °F | ASTM D3418 |
3M Dyneon™ PVDF 32008/0003 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesExcellent low flame and low smoke pe.. |
|||
Melting Point | 168 °C | 334 °F | Kofler |
Lubrizol Estane® 58437 Thermoplastic Polyurethane Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi.. |
|||
Melting Point | 168 °C | 334 °F | ISO 11357 |
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 168 °C | 334 °F | ISO 11357 |
Polyram RamOfin PPH343T4BK11 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat resistant polypropylene for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 168 °C | 334 °F | ASTM D3418 |
3M Dyneon™ PVDF 31008/0003 Polyvinylidene Fluoride
(discontinued **) 3M™ Dyneon™ PVDF 31008/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31008/0003 also has a very low brittleness temperatu.. |
|||
Melting Point | 168 °C | 334 °F | ASTM D3418 |
3M Dyneon™ PVDF 31008/0009 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesExcellent low flame and low smoke .. |
|||
Melting Point | 168 °C | 334 °F | ASTM D3418 |
3M Dyneon™ PVDF 32008/0000 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesInformation provided by Dyneon, A 3M.. |