Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 141 - 145 °C | 285 - 293 °F | ASTM D3418 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |