Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from .. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + TLS Polyethylene Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i.. |
|||
Melting Point | 130 °C | 266 °F | |
Plastcom SLOVALEN PC 79 GF 20 PP, 20% glass fibre, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 - REG PE Multicoloured fine OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 133 °C | 266 - 271 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Melting Point | 130 - 133 °C | 266 - 271 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cestidur™ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 130 °C | 266 °F | ASTM D3417 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Melting Point | 130 - 133 °C | 266 - 271 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Melting Point | 130 °C | 266 °F | Exxon Method |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |
|||
Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
FKuR Kunststoff Terralene® WF 5525 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
FKuR Kunststoff Terralene® WF 6534 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melting Point | 130 °C | 266 °F | |
Hyosung Topilene C500H PP C500H Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melting Point | 130 °C | 266 °F | |
Hyosung Topilene C600H2 PP C600H2 Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melting Point | 130 °C | 266 °F | fusing temperature |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer Features: SEETEC M1400 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1400 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer Features: SEETEC M1600 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1600 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Melting Point | 130 °C | 266 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC PB150 HDPE Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stre.. |
|||
Melting Point | 130 - 173 °C | 266 - 343 °F | |
Indium Corp. Indalloy 101 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DIN 53 736 |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Melting Point | 130 °C | 266 °F | Dow Method (DSC) |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Melting Point | 130 °C | 266 °F | Dow Method (DSC) |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Melting Point | 130 °C | 266 °F | ASTM D3418 |
ExxonMobil HD 6605.70 Injection Molding Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Melting Point | 130 - 132 °C | 266 - 270 °F | crystalline; DSC |
Total Xsene® XS10 Orange YCF HDPE, pipe FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 ORANGE YCF is a high performance .. |
|||
Melting Point | 130 °C | 266 °F | |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: .. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC R7700 Polypropylene, Random Copolymer Features: Seetec R7700 is designed for the extrusion of fibers with the spunbond technology. This grade is characterized by narrow MWD and good processability. SEETEC R7700 meets the FDA requirement.. |