Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1435 - 1446 °C | 2615 - 2635 °F | |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Melting Point | 1435 - 1446 °C | 2615 - 2635 °F | |
Special Metals Nickel 201 Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C)... |
|||
Melting Point | 1435 - 1446 °C | 2615 - 2635 °F | |
Special Metals Nickel 205 Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic.. |
|||
Melting Point | 1435 - 1446 °C | 2615 - 2635 °F | |
Special Metals Nickel 212 Wrought nickel strengthened with an added manganese. Used for electrical and electronic applications such as lead wires, supporting components in lamps and cathode-ray tubes, and electrodes in glow.. |
|||
Melting Point | 1435 °C | 2615 °F | |
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
Melting Point | 1435 - 1505 °C | 2615 - 2741 °F | |
Special Metals UDIMET® Alloy 250 Maraging Steel A high-strength, maraging steel of iron and nickel with additions of molybdenum and titanium. It has the strength of standard 18Ni (250) maraging steel but the advantages of containing less molybde.. |
|||
Melting Point | 1435 - 2002 °C | 2615 - 3635 °F | |
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
Melting Point | 1435 - 1446 °C | 2615 - 2635 °F | |
Carlson C 201 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |