Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 124 °C | 255 °F | Internal method |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
Melting Point | 124 °C | 255 °F | Internal method |
Polimeri Europa Flexirene® MR 50 A Linear Low Density Polyethylene Flexirene MR 50 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Melting Point | 124 °C | 255 °F | 10°C/min; ISO 11357-1/-3 |
DSM Yparex® 7102 Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Melting Point | 124 °C | 255 °F | ISO 11357-3 |
Total Finathene® LL 6010 FH 18P LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Melting Point | 124 °C | 255 °F | |
M. Holland Company MAGMA® LL1091 LLDPE
(discontinued **) Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | 124 °C | 255 °F | 10°C/min; ISO 11357-1/-3 |
Yparex 8403 S Polyolefin Adhesive Resin The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melting Point | 124 °C | 255 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M70 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High flowFast cycle timesExcellent surface finishingTypical Applications: Complex/Intricate products, high volume/short cyc.. |
|||
Melting Point | >= 124 °C | >= 255 °F | ISO 11357/03 |
Borealis Borstar® FB2230 LLDPE for Film Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Melting Point | 124 °C | 255 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3001.32 Cast Film Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Melting Point | 124 °C | 255 °F | ASTM D3418 |
ExxonMobil LL 6100.17 Injection Molding Resin Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in .. |
|||
Melting Point | 124 °C | 255 °F | Equate Test Method |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |
|||
Melting Point | 124 °C | 255 °F | Equate Test Method |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow ATTANE™ 4404G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by.. |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by.. |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow ELITE™ 5100G Enhanced Polyethylene Resin ™ 5100G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers excellent impact strength, good tensile and puncture properties for thick and thin gauge industrial and consume.. |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de.. |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f.. |
|||
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Melting Point | 124 °C | 255 °F | |
Arkema Group Orevac® 18303S Maleic Anhydride modified LLDPE LLDPE base Composition: PE / Adh./ EVOH Applications:Flooring Heating TubeInformation provided by Arkema Group |
|||
Melting Point | 124 °C | 255 °F | D.S.C. method |
Arkema Group Orevac® OE807 Maleic Anhydride modified LLDPE Orevac® OE807 resin is a maleic anhydride modified LLDPE designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between the layers. Orevac® OE807 is characte.. |
|||
Melting Point | 124 °C | 255 °F | ASTM-D3418 |
Braskem RD34U3 LLDPE Rotomolding Polyethylene The resin RD34U3 is a linear low-density polyethylene, 1-butene based, with excellent processability and a good balance of stiffness and impact strength. It contains long term UV6 stabilization and .. |
|||
Melting Point | 124 °C | 255 °F | D.S.C. method |
Arkema Group Orevac® 18302 Maleic Anhydride modified LLDPE Orevac® 18302 resin is a maleic anhydride modified LLDPE designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between the layers.Information provided by Arke.. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Melting Point | 124 °C | 255 °F | Exxon Method |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Melting Point | 124 °C | 255 °F | ASTM D3417 |
Total Finacene® BM359SG HDPE, blow molding
(Unverified Data**) FINACENE® BM359 SG has been especially designed for the manufacture of blow moulded bottles (up to 5 liters) with a superior surface gloss and contact transparency. It is recommended either in mono.. |
|||
Melting Point | 124 - 128 °C | 255 - 262 °F | Average value: 127 °C Grade Count:5 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Melting Point | 124 - 135 °C | 255 - 275 °F | Average value: 129 °C Grade Count:19 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |