Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 122 °C | 252 °F | Internal method |
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 1327CA Blown Film Resin
(discontinued **) Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Melting Point | 122 °C | 252 °F | Exxon Method |
ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for effici.. |
|||
Melting Point | 122 °C | 252 °F | ISO 11357-3 |
Total Finathene® LL 4010 FH 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
(discontinued **) Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Melting Point | 122 - 155 °C | 252 - 311 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
Melting Point | 122 - 160 °C | 252 - 320 °F | |
Indium Corp. Indalloy 93 Bismuth-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 122 °C | 252 °F | DSC |
Silon Tabond 3044 Adhesive Resin TABOND 3044 is LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Str.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 5100.09 Compounding Resin Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending .. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 5252.09 Compounding Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2021D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2045G Linear Low Density Polyethylene DOWLEX™ 2045G resin is designed for the production of a wide variety of industrial and consumer films (though it is not recommended for silage stretch film). The product also delivers very good pr.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2047G Linear Low Density Polyethylene For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2071D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2078G Linear Low Density Polyethylene Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2267G Linear Low Density Polyethylene A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow FLEXOMER™ ETS-9066 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2021D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Internal Measurement |
Bapolene® 83 Polyethylene Terephthalate Applications: Personal care, household, liquor and food containers. All data is based on molded plaques. |
|||
Melting Point | 122 °C | 252 °F | |
DuPont Fusabond® MX110D Linear Low Density Polyethylene
(discontinued **) Typical Use: CompatibilizerCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideNatural fiber wood-plastic comp.. |
|||
Melting Point | 122 °C | 252 °F | |
DuPont Fusabond® MD226D Linear Low Density Polyethylene
(discontinued **) Typical Use: CompatibilizerCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideNatural fiber wood-plastic comp.. |