Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1352 °C | 2465 °F | |
Universal Wire Works No. 21 Cobalt Alloy Welding Wire Universal No. 21 is a cobalt-chromium-molybdenum alloy designed for covered electrode, TIG, MIG, hard surfacing applications. The work-hardening characteristics, high ductility properties, excellent.. |
|||
Melting Point | <= 1352 °C | <= 2465 °F | |
Weartech International WT-800 Cobalt Hardfacing & Wear Resistant Alloy Applications: Magnetic tape heads, valves, extruder barrelsInformation provided by Weartech International |