Thermal Properties Metric English Comments
Melting Point 1324 - 1370 °C
2415 - 2500 °F
Carlson GOC 276 Nickel-Molybdenum-Chromium
General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in ..