Thermal Properties Metric English Comments
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.7 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 4.8 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6K 1.6 mm thick sheet
13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6K 12.7 or 22.2 mm plate
13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 3.2 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Melting Point 1265 - 1354 °C
2309 - 2469 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate, aged 3 hours at 816°C