Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 110 °C | 230 °F | Internal method |
Polimeri Europa Riblene® MM 20 R Low Density Polyethylene - Injection Molding Riblene MM 20 R is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MM 20 R are characterized by a high flexibility.Main Applications: Riblene MM 20 R is suitable for i.. |
|||
Melting Point | 110 °C | 230 °F | |
Reade Advanced Materials Gallium Nitrate (Ga(NO3)3·XH2O ) Sometimes used as an antihypercalcemic agent.Information provided by Reade Advanced Materials. |
|||
Melting Point | 110 - 200 °C | 230 - 392 °F | Average value: 151 °C Grade Count:29 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 503.LN Foams and Compounding Resin
(discontinued **) LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 513.48 Molding, Extrusion and Compounding Resin
(discontinued **) LD 513.48 is a medium MI, low density polyethylene resin designed for use in compounds and masterbatches where its properties ensure improved processability and uniform dispersion of additives. The.. |
|||
Melting Point | 110 °C | 230 °F | Exxon Method |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Melting Point | 110 °C | 230 °F | NOVA |
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin
(discontinued **) NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat.. |
|||
Melting Point | 110 - 220 °C | 230 - 428 °F | Average value: 214 °C Grade Count:19 |
Overview of materials for Nylon 6 Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Melting Point | 110 - 164 °C | 230 - 327 °F | Huntsman/TMA |
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | |
Fine Organics FINAWAX VL Lubricant Additive Applications: Antiblock agent for soft PVC calendered films/sheets, specially for printed films with antiblocking properties.Information provided by Fine Organics |
|||
Melting Point | 110 °C | 230 °F | DSC |
LG Chemical LUTENE BB0808 LDPE Blown Film Grade Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc.. |
|||
Melting Point | 110 °C | 230 °F | DSC |
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film Description: LUTENE FB3000 is mainly intended for the extrusion of blown film with high mechanical property for the clarity bags in all thickness. LUTENE FB3000 have high mechanical property and ena.. |
|||
Melting Point | 110 - 130 °C | 230 - 266 °F | |
LG Chemical LUTENE XL2700BK PE Compound Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventi.. |
|||
Melting Point | 110 - 125 °C | 230 - 257 °F | |
Hong Kun Group AO 1010 Antioxidant CAS No. 6683-19-8All information provided by Hongkun Group |
|||
Melting Point | 110 °C | 230 °F | ASTM D3418 |
LyondellBasell Microthene® G MN72200 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melting Point | 110 - 143 °C | 230 - 289 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN .. |
|||
Melting Point | 110 °C | 230 °F | DSC |
LG Chemical LUTENE FB0800 LDPE Blown Film Description: LUTENE FB0800 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of greenhouse film. LUTENE FB0800 have the excellent mechanical proper.. |
|||
Melting Point | 110 - 125 °C | 230 - 257 °F | |
Suqian Unitechem Antioxidant 1010 Chemical Name: Tetrakis [methylene-3-(3,5-di-tert-butyl-4-hydroxyphenyl-propionate)]methaneCAS NO.: 6683-19-8Molecular Formula: C73H108O12Properties: The product takes on the appearance of white pow.. |
|||
Melting Point | 110 °C | 230 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ LD1902F Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactContains 1400 ppm slip content and 2400 ppm antiblocking contentRecommended Applications:G.. |
|||
Melting Point | 110 °C | 230 °F | ISO 11357-3 |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Melting Point | 110 °C | 230 °F | ISO 11357-3 |
Borealis FT3200 Low Density Polyethylene FT3200 is a Low Density Polyethylene for Film Extrusion. Applications heavy-duty bags, shrink film, construction films, and agricultural films. FT3200 contains no additives.Information provided by.. |
|||
Melting Point | 110 - 155 °C | 230 - 311 °F | ISO 3146 |
Borealis Steripeel™ WD165CF PO Compound for Sterilizable Peelable Film Applications Steripeel WD165CF is a non-formulated film resin, specially developed for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WD165CF is suitable for various peelable.. |
|||
Melting Point | 110 - 115 °C | 230 - 239 °F | DSC |
EMS-Griltech Griltex® 8E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
EMS-Griltech Griltex® D 1694A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Melting Point | 110 °C | 230 °F | Exxon Method |
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym.. |