Thermal Properties Metric English Comments
Melting Point 1246 - 1356 °C
2275 - 2473 °F
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or ..