Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 107 °C | 224 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |
|||
Melting Point | 107 °C | 224 °F | Dow Method (DSC) |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |