Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 Hard, 1.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 MH8, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way)..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard, 1.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): ..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 Annealed
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): ..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way)..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Melting Point 1195 - 1325 °C
2183 - 2417 °F
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..