Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 92.0 °C | 198 °F | Internal Method |
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: .. |
|||
Melting Point | 92.0 °C | 198 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 30E699 Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 92.0 °C | 198 °F | Exxon Method |
ExxonMobil Escorene® LD-705 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |
|||
Melting Point | 92.0 - 121 °C | 198 - 250 °F | |
Indium Corp. Indalloy 63 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 92.0 °C | 198 °F | Freezing Point via DSC/ASTM D3418 |
DuPont 20 Series DPE 20 Specialty Polyethylene Resin DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex.. |
|||
Melting Point | 92.0 °C | 198 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Melting Point | 92.0 °C | 198 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go.. |
|||
Melting Point | 92.0 °C | 198 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 92.0 °C | 198 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res.. |
|||
Melting Point | 92.0 °C | 198 °F | TRN-14 |
Tipco Tipcolite® TPF 1312 - Unreinforced Thermoset Phenolic Resin, 21 mm Norton Flow with 13% Hexamine Unreinforced Phenolic Resin having 21mm Norton Flow, in Powder FormApplications: General PurposeProcessing: General PurposeInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Melting Point | 92.0 °C | 198 °F | ISO 11357 |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Melting Point | 92.0 °C | 198 °F | DSC; ASTM D3418 |
DuPont Appeel® LSR20D745 Lidding Sealant Resin Appeel® LSR20D745 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu.. |
|||
Melting Point | 92.2 °C | 198 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil EXACT™ 3128 Plastomer for Blown Film Applications Product Description: Exact 3128 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It is designed fro both monolayer and multilayer coextruded .. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3418, ISO 3146 |
DuPont™ Appeel® 20D855 Ethylene Acrylate DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 22E757 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3418, ISO 3146 |
DuPont™ Entira® AS500 Ionomer Resin Entira™ AS MK400 is used to lower the static decay time and surface resistivity of polyolefins and other polymers. Entira™ AS MK400 can be precompounded or dry blended into polymers for extrusion,.. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3418, ISO 3146 |
DuPont™ Entira® ASSD100 Ionomer Resin DuPont™ Entira™ AS SD100 is an extremely hygroscopic ionomer resin that is supplied as free flowing pellets. Entira™ AS SD100 is used to lower the static decay time and surface resistivity of LD.. |
|||
Melting Point | 92.0 °C | 198 °F | DTA |
DuPont™ Surlyn® 9650 Ionomer Resin, Zinc Surlyn® 9650 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 92.0 °C | 198 °F | DTA |
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 92.0 °C | 198 °F | DTA |
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 92.0 °C | 198 °F | 10°C/min |
Arkema Group Evatane® 1040 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and high mechanical properties. Examples: thin stretch film for food packaging, coex.. |
|||
Melting Point | 92.0 °C | 198 °F | DSC |
Arkema Group LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 14 MGC 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the Methyl Acrylate content, LOTRYL® 14 MGC 02 is a polymer o.. |
|||
Melting Point | 92.0 °C | 198 °F | ASTM D3417, ISO 3146 |
DuPont™ Surlyn® 1707 Sodium Ionomer Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Melting Point | 92.0 °C | 198 °F | Exxon Method |
ExxonMobil Escorene® LD-702 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |
|||
Melting Point | 92.0 °C | 198 °F | Eutectic |
Indium Corp. Indalloy 197 Bismuth Solder Alloy Information Provided by Indium Corporation |