Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1070 - 1080 °C | 1950 - 1980 °F | |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Melting Point | <= 1070 °C | <= 1950 °F | |
Weartech International WT-50 Nickel Hardfacing & Wear Resistant Alloy Applications: liners, thrust shoes, bushings, cages and other valve components for nuclear applicationsInformation provided by Weartech International |