Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 937 °C | 1720 °F | |
Mateck Germanium (Ge) Optical crystals |
|||
Melting Point | 935 °C | 1720 °F | |
American Elements Praseodymium Nanoparticles General DescriptionPraseodymium (Pr) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Praseodymium Particles are typically 10 - 45 nanometers (nm) wit.. |
|||
Melting Point | 935 °C | 1720 °F | |
Goodfellow Copper 70/Titanium 30 Alloy Information provided by Goodfellow. |