Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 75.0 °C | 167 °F | |
M. Holland Company MAGMA® LM372-A LLDPE
(discontinued **) Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Melting Point | 75.0 °C | 167 °F | ISO 11357-3 |
Total Evatane® 28 - 03 HDPE, blown film
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Melting Point | 75.0 °C | 167 °F | Exxon Method |
ExxonMobil Escorene® LD-768 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 27.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Melting Point | 75.0 - 85.0 °C | 167 - 185 °F | |
Fine Organics FINALUX GH 5 Lubricant Additive Applications: Internal lubricant for rigid PVC injection molded fittings, calendered, blown films/sheets, PVC bottles and other Sn-mercaptide stabilized rigid PVC products. Excellent synergistic co.. |
|||
Melting Point | 75.0 - 118 °C | 167 - 244 °F | |
Indium Corp. Indalloy 59 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 75.0 °C | 167 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3130 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 75.0 °C | 167 °F | by DSC; ASTM D3418 |
Westlake EMAC® SP2268 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2268 is a 24% EMA copolymer designed for extrusion coating, tie-layers, compounding, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Melting Point | 75.0 °C | 167 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3810 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 75.0 °C | 167 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Melting Point | 75.0 - 85.0 °C | 167 - 185 °F | DSC |
EMS-Griltech Griltex® D 1531E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 75.0 - 85.0 °C | 167 - 185 °F | DSC |
EMS-Griltech Griltex® D 1582E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 75.0 - 85.0 °C | 167 - 185 °F | DSC |
EMS-Griltech Griltex® D 1666A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 75.0 °C | 167 °F | Peak Melting Temperature; ISO 11357-3 |
ExxonMobil EXACT™ 8210 Plastomer for Multilayer Film Applications Product Description: Exact 8210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications req.. |
|||
Melting Point | 75.0 °C | 167 °F | DSC |
Arkema Group OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer OREVAC® 18211 is maleic anhydride grafted EVA copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. ORE.. |
|||
Melting Point | 75.0 °C | 167 °F | ASTM-D3418 |
Braskem Evateno® HM 2528 EVA Hot Melt Copolymer Evateno® HM 2528 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, low molecular weight, and good compatibility with other thermoplastic and elastomeric resins, and it.. |
|||
Melting Point | 75.0 °C | 167 °F | DSC |
Arkema Group OREVAC® 18390 Maleic Anhydride Modified Polyethylene OREVAC® 18390 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Melting Point | 75.0 °C | 167 °F | |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | 75.0 - 128 °C | 167 - 262 °F | Average value: 113 °C Grade Count:36 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Melting Point | 75.0 °C | 167 °F | by DSC; ASTM D3418 |
Westlake EMAC® SP2403 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2403 is a 24% EMA copolymer designed for extrusion coating, tie-layers, compounding, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Melting Point | 75.0 °C | 167 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 75.0 °C | 167 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Appeel® LSR 1181 Modified EVA Lidding Sealing Resin Appeel® 1181 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |