Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 72.2 °C | 162 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil ESCOR™ AT 320 Blown Film Resin
(discontinued **) ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical |
|||
Melting Point | 72.2 °C | 162 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil ESCOR™ AT 320 Cast Film Resin
(discontinued **) ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical |
|||
Melting Point | 72.0 °C | 162 °F | ISO 11357-3 |
Total Evatane® 28 - 05 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 120 to 150.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Melting Point | 72.0 °C | 162 °F | Exxon Method |
ExxonMobil Escorene® LD-761 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Appl.. |
|||
Melting Point | 72.0 °C | 162 °F | Exxon Method |
ExxonMobil Escorene® LD-769 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer designed for high filler acceptance. Compounds produced from this resin have excellent flexibility and toughness.Appl.. |
|||
Melting Point | 72.0 °C | 162 °F | Exxon Method |
ExxonMobil Escorene® MV-02520 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An experimental, very high flow, 20% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 72.0 - 135 °C | 162 - 275 °F | Average value: 127 °C Grade Count:49 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Melting Point | 72.0 - 76.0 °C | 162 - 169 °F | |
Hong Kun Group ITX Additive Chemical Name: 2-(2,4-Diaminophenoxy)ethanol dihydrochlorideCAS No. 5495-84-1All information provided by Hongkun Group |
|||
Melting Point | 72.0 °C | 162 °F | Eutectic |
Indium Corp. Indalloy® 162 In-Bi Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 72.0 - 113 °C | 162 - 235 °F | |
Indium Corp. Indalloy 55 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 72.0 - 76.0 °C | 162 - 169 °F | |
Suqian Unitechem 1,2,2,6,6-Pentamethyl-4-piperidinol Chemical Name: 1,2,2,6,6-Pentamethyl-4-piperidinolCAS NO.: 2403-89-6Molecular Formula: C10H21NOUses: It is an important intermediate of hindered amine light stabilizer and synthetic hindered amine l.. |
|||
Melting Point | 72.0 °C | 162 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 4170 Reactive Ethylene Terpolymer (RET) A reactive ethylene terpolymer (RET) that can be used to modify the properties of asphalt binder used in paving.Elvoy® 4170 is the most chemically reactive of the terpolymers manufactured by DuPont.. |
|||
Melting Point | 72.0 °C | 162 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® PTW Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melting Point | 72.0 °C | 162 °F | ASTM D3417 |
DuPont Elvax® 3182-2 Ethylene Vinyl Acetate DuPont™ Elvax® 3182-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applicat.. |
|||
Melting Point | 72.0 °C | 162 °F | Freezing Point; ASTM D3418 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Melting Point | 72.2 °C | 162 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications Product Description: Exact 4056 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin can be used in blends with polyolefins to improve.. |
|||
Melting Point | 72.2 °C | 162 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low .. |
|||
Melting Point | 72.2 °C | 162 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 220 ExCo Ethylene Methyl Acrylate Product Description: Product Description: Optema TC 220 is an ethylene methyl acrylate copolymer, which can be used for making alloys, blends and compounds or be injection molded where softness and .. |
|||
Melting Point | 72.0 °C | 162 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8411 Polyolefin Elastomer Description: Engage® 8411 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable injection molded industrial and consumer goods and compression molded gask.. |
|||
Melting Point | 72.0 °C | 162 °F | DSC |
Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a poly.. |
|||
Melting Point | 72.0 °C | 162 °F | DSC |
Arkema Group LOTRYL® 37 EH 550 Copolymer Ethylene - Acrylic Ester LOTRYL 37 EH 550 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. Co-monomer content is 37% in weight. LOTRYL 37 EH 550 is particula.. |
|||
Melting Point | 72.0 °C | 162 °F | DSC |
Arkema Group EVATANE® 28-05 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-05 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-05 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | 72.2 - 102 °C | 162 - 216 °F | Average value: 87.9 °C Grade Count:17 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an.. |
|||
Melting Point | 72.0 - 104 °C | 162 - 219 °F | Average value: 89.8 °C Grade Count:14 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |
|||
Melting Point | 72.0 °C | 162 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® PT Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer
(discontinued **) Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melting Point | 72.0 °C | 162 °F | Exxon Method |
ExxonMobil Escorene® UL-7760 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 72.0 °C | 162 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® AS Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer
(discontinued **) Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |