Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 71.1 °C | 160 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 767.MJ Blown Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Melting Point | 71.1 °C | 160 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Melting Point | 71.0 - 74.0 °C | 160 - 165 °F | |
Hong Kun Group DETX Additive CAS No. 82799-44-8All information provided by Hongkun Group |
|||
Melting Point | 71.0 - 93.0 °C | 160 - 199 °F | TMA Melt Range |
Huntsman IROGRAN® CA 117-200 DP TPU-Polyester Polyester-based TPUs that are specially designed for adhesives applications where high green strength and a fast crystallization rate are essential qualities.Information provided by Alliance Polymer.. |
|||
Melting Point | 71.0 - 88.0 °C | 160 - 190 °F | TMA Melt Range |
Huntsman IROGRAN® PS 456-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Melting Point | 71.0 °C | 160 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5004 1000 Micron EVA Powder Description: ICOFLO 510-5004 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Melting Point | 71.0 °C | 160 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny.. |
|||
Melting Point | 71.0 - 88.0 °C | 160 - 190 °F | |
Indium Corp. Indalloy 160-190 Fusible Bismuth Alloy Information Provided by Indium Corporation |
|||
Melting Point | 71.0 °C | 160 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 71.1 °C | 160 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® UL 8705 Adhesive Application Resin Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has .. |
|||
Melting Point | 71.1 °C | 160 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® UL 8705E Adhesive Application Resin Escorene Ultra UL 8705 is a relatively low viscosity, 29% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has go.. |
|||
Melting Point | 71.0 °C | 160 °F | ASTM D3418, ISO 3146 |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Melting Point | 71.0 °C | 160 °F | ASTM D3418, ISO 3146 |
DuPont™ Fusabond® C190 Polymer Modifier DuPont™ Fusabond® C190 is a anhydride modified ethylene vinyl acetate copolymer. Uses: Adhesives Pipe Coating Polymer Modifier |
|||
Melting Point | 71.0 °C | 160 °F | ASTM D3418, ISO 3146 |
DuPont™ Fusabond® C250 Polymer Modifier DuPont™ Fusabond® C250 is a modified ethylene vinyl acetate copolymer. Used as an adhesion promoter and coupling agent. |
|||
Melting Point | 71.0 °C | 160 °F | DSC |
Arkema Group EVATANE® 28-25 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-25 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | 71.0 °C | 160 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Melting Point | 71.0 - 225 °C | 160 - 437 °F | Average value: 155 °C Grade Count:57 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Melting Point | 71.0 °C | 160 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® CM576 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® CM576 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low .. |
|||
Melting Point | 71.0 °C | 160 °F | |
DuPont Fusabond® MC190D Ethylene Vinyl Acetate (28% VA)
(discontinued **) Typical Use: Adhesion promoterCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideAvailability: North AmericaI.. |
|||
Melting Point | 71.0 °C | 160 °F | |
DuPont Fusabond® MC250D Ethylene Vinyl Acetate (28% VA)
(discontinued **) Typical Use: Adhesion promoterCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideAvailability: North AmericaI.. |
|||
Melting Point | 71.0 °C | 160 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued 12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des.. |