Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 70.0 °C | 158 °F | Exxon Method |
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Melting Point | 70.0 °C | 158 °F | DSC |
DuPont™ Surlyn® 9320W Ionomer Resin, Zinc
(discontinued **) Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc.. |
|||
Melting Point | 70.0 - 80.0 °C | 158 - 176 °F | |
Fine Organics FINALUX G 211 Lubricant Additive Applications: External lubricants for rigid and soft PVC, specially for Ba-Cd stabilized PVC products.Information provided by Fine Organics |
|||
Melting Point | 70.0 - 80.0 °C | 158 - 176 °F | |
Fine Organics FINALUX G 411 Lubricant Additive Applications: Compatible lubricant for rigid PVC preferable for use in glass clear rigid PVC articles, lubricant for duroplast.Information provided by Fine Organics |
|||
Melting Point | 70.0 - 102 °C | 158 - 216 °F | |
Indium Corp. Indalloy 43 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 123 °C | 158 - 253 °F | |
Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 80.0 °C | 158 - 176 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 104 Linear Thermoplastic Polyurethane Pearlbond™ 104.is a linear, aromatic polyurethane, supplied in form of small white or slightly yellowish granules, which combines a high crystallisation rate with a high thermoplasticity level... |
|||
Melting Point | 70.0 - 73.0 °C | 158 - 163 °F | |
Indium Corp. Indalloy 22 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 73.0 °C | 158 - 163 °F | |
Indium Corp. Indalloy 23 Bismuth Solder Alloy Non-electrical solder for low-ambient temperatureInformation Provided by Indium Corporation |
|||
Melting Point | 70.0 - 73.0 °C | 158 - 163 °F | |
Indium Corp. Indalloy 24 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 - 78.0 °C | 158 - 172 °F | |
Indium Corp. Indalloy 26 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 70.0 °C | 158 °F | Eutectic |
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy Lowest melting point solder. Good fusible alloy used for lens blocking.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 70.0 °C | 158 °F | |
Synergy Polymers Ultra Purge P-O Ultra Purge is a specially designed cleaning compound that comes premixed and ready-to-use in pellet form. It cleans black specks and deposits from screws, barrels, nozzle, hot runners and heads of .. |
|||
Melting Point | 70.0 - 76.0 °C | 158 - 169 °F | |
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent Unsaturated fatty primary amide derived from oleic acid.One of the major uses of oleamide is as a slip agent in polyethylene films. It functions by migrating to the film surface in a microscopic coa.. |
|||
Melting Point | 70.0 - 75.0 °C | 158 - 167 °F | |
Solvay ALKAMULS® 504/V Surfactant Chemical Name: ETHYLENE GLYCOL DISTEARATECAS: 627-83-8Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Ethylene glycol distearate is widely used in cosmetics as pearl.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 4924 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melting Point | 70.0 °C | 158 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3180 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3180 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 70.0 °C | 158 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Bynel® 1124 Modified EVA Adhesive Resin Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3417 |
DuPont Elvax® 3180Z Ethylene Vinyl Acetate DuPont™ Elvax® 3180Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applicati.. |
|||
Melting Point | 70.0 °C | 158 °F | Exxon Method |
ExxonMobil EXACT™ 4053 Cast Plastomer Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Melting Point | 70.0 °C | 158 °F | Peak Melting, Exxon Method |
ExxonMobil EXACT™ 4053 Plastomer for Film Applications Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Melting Point | 70.0 °C | 158 °F | DSC |
DuPont™ Surlyn® 8320 Ionomer Resin, Sodium Surlyn® 8320 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. This very low modulus sod.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3418, ISO 3146 |
DuPont™ Surlyn® 9320 Zinc Ionomer Surlyn® 9320 is a zinc ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 9320 thermoplastic resin .. |
|||
Melting Point | 70.0 °C | 158 °F | Dow Method |
Dow AFFINITY™ GA 1950 Polyolefin Plastomer (POP) AFFINITY™ GA 1950 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3418, ISO 3146 |
DuPont™ Surlyn® 6320 Magnesium Ionomer Surlyn® 6320 is a magnesium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 6320 thermoplastic r.. |
|||
Melting Point | 70.0 °C | 158 °F | DSC |
Arkema Group EVATANE® 28-40 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-40 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-40 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | 70.0 - 103 °C | 158 - 217 °F | Average value: 89.8 °C Grade Count:9 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |
|||
Melting Point | 70.0 °C | 158 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® CM4875 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® CM4875 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low.. |
|||
Melting Point | 70.0 °C | 158 °F | |
Reade Advanced Materials Wood's Metal Alloy (Sn + Pb + Bi + Cd) Description: A low melting fusible alloy.Various granulations are available. Used in heating baths in laboratories, antifriction metals, and solders.Information provided by Reade Advanced Materials.. |