Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 66.7 - 216 °C | 152 - 421 °F | Average value: 108 °C Grade Count:43 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Melting Point | 66.7 °C | 152 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil ESCOR™ AT 325 Molding, extrusion and compounding resin
(discontinued **) ESCOR AT 325 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials. It has the highest melt index and the lowest modulus of all the Escor Acid Terpoly.. |