Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane Pearlbond™ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melting Point | >= 63.0 °C | >= 145 °F | |
Hong Kun Group AO 1035 Antioxidant Chemical Name: 2,2'-Thio-bis{ethyl-B-(3,5-ditertbutyl-4-hydroxyphenyl)}-propionateCAS No. 41484-35-9All information provided by Hongkun Group |
|||
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane Pearlbond™ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve.. |
|||
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 501 Linear Thermoplastic Polyurethane Pearlbond™ 501 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |
|||
Melting Point | 63.0 °C | 145 °F | ASTM D3417 |
DuPont Elvax® 150 Ethylene Vinyl Acetate DuPont™ Elvax® 150 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 150 resins can be used for the following applications: molding, compoundin.. |
|||
Melting Point | 63.0 °C | 145 °F | ASTM D3417 |
DuPont Elvax® 150W Ethylene Vinyl Acetate DuPont™ Elvax® 150W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Melting Point | 63.0 °C | 145 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® HP771 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melting Point | 63.0 °C | 145 °F | Freezing Point; ASTM D3418, ISO 3146 |
DuPont™ Elvax® 3155 Ethylene Vinyl Acetate DuPont™ Elvax® 3155 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 31.. |
|||
Melting Point | 63.0 °C | 145 °F | Dow Method |
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in .. |
|||
Melting Point | >= 63.0 °C | >= 145 °F | Wax Infiltrated; ASTM D3418 |
ALM PS 200 Prototyping Polymer Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castfor.. |
|||
Melting Point | 63.0 °C | 145 °F | DSC |
Arkema Group EVATANE® 33-25 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-25 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | >= 63.0 °C | >= 145 °F | Wax |
3D Systems CastForm™ PS Plastic for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsCreate patterns directly rather than through indirect methodsComplex investment casting patternsReactive metals like titaniumLo.. |
|||
Melting Point | 63.0 - 67.0 °C | 145 - 153 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 521 Linear Thermoplastic Polyurethane Pearlbond™ 521 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl.. |
|||
Melting Point | 63.0 °C | 145 °F | ASTM D3417 |
DuPont Elvax® 150W-LG Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 150W-LG is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent th.. |