Polymer Property : Melting Point = 135 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 57.0 - 67.0 °C
135 - 153 °F
Fine Organics FINALUX G 120 Lubricant Additive
Applications: Lubricant for rigid PVC fittings, films and other Sn-mercaptide stabilized articles. Suitable for PVC cable compounds.Information provided by Fine Organics
Melting Point 57.0 °C
135 °F
LG Chemical LC370 Polyolefin Elastomer for Polymer Modification
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio..
Melting Point 57.0 - 65.0 °C
135 - 149 °F
Indium Corp. Indalloy 140 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 57.0 °C
135 °F
Freezing Point; ASTM D3418
DuPont™ Elvax® 3178Z Ethylene Vinyl Acetate
DuPont™ Elvax® 3178Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3..
Melting Point 57.0 °C
135 °F
Freezing Point; ASTM D3418, ISO 3146
DuPont™ Elvax® 3190A Ethylene Vinyl Acetate
DuPont™ Elvax® 3190A is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3..
Melting Point 57.0 °C
135 °F
DSC
Arkema Group EVATANE® 33-400 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-400 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-400 is stabilized with antioxidants. The High Vinyl Acetate ..